Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.13 MPa @Strain 6.80 %, Temperature 120 °C |
599 psi @Strain 6.80 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |