Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 40.4 MPa @Strain 4.21 %, Temperature 150 °C |
5860 psi @Strain 4.21 %, Temperature 302 °F |
ISO 527 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |
|||
Tensile Stress | 40.4 MPa @Strain 1.59 %, Temperature 120 °C |
5860 psi @Strain 1.59 %, Temperature 248 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |