Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 39.58 MPa @Strain 2.60 %, Temperature 180 °C |
5741 psi @Strain 2.60 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK549 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Information provided by DuPont Performance Polymers |