Polymer Property : Tensile Stress = 553 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 3.81 MPa

@Strain 100 %
553 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® F02-137B TPE, Halogen Free Extrusion Grade
Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to..
Tensile Stress 3.81 MPa

@Strain 173.97 %,
Temperature 120 °C
553 psi

@Strain 173.97 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers