Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 37.99 MPa @Strain 0.300 %, Temperature 0.000 °C |
5510 psi @Strain 0.300 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te.. |
|||
Tensile Stress | 38.0 MPa @Strain 300 % |
5510 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 6055D Thermoplastic Polyurethane Elastomer Zythane™ 6055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 38.0 MPa @Strain 300 % |
5510 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 7055D Thermoplastic Polyurethane Elastomer Zythane™ 7055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | >= 38.0 MPa @Strain 300 % |
>= 5510 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 272D Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Stress | 38.0 MPa @# of Cycles 1.00e+6 , Temperature 180 °C |
5510 psi @# of Cycles 1.00e+6 , Temperature 356 °F |
|
BASF Ultrason E 2010 G6 30% Glass Filled PES Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |