Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 55.9 MPa @Strain 1.93 %, Temperature 23.0 °C |
8110 psi @Strain 1.93 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |