Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.78 MPa @Strain 100 % |
548 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3875 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 3.78 MPa @Strain 300 % |
548 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® S4750 TPE, PS Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesSporting GoodsInformation from Alliance Polymers & Services, Distributor of Nantong .. |
|||
Tensile Stress | 3.78 MPa @Strain 130.87 %, Temperature 120 °C |
548 psi @Strain 130.87 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |
|||
Tensile Stress | 3.78 MPa @Strain 5.25 %, Temperature 90.0 °C |
548 psi @Strain 5.25 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 3.78 MPa @Strain 5.25 %, Temperature 90.0 °C |
548 psi @Strain 5.25 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |