Mechanical Properties Metric English Comments
Tensile Stress 54.89 MPa

@Strain 3.86 %,
Temperature 23.0 °C
7961 psi

@Strain 3.86 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6  (Unverified Data**)
15% Glass Reinforced Heat Stabilized Polyamide 6 Zytel BM73G15THS is a 15% glass fiber reinforced heat stabilized lubricated toughened polyamide 6 for blow molding.Information provided by DuPont Per..
Tensile Stress 54.89 MPa

@Strain 1.50 %,
Temperature 100 °C
7961 psi

@Strain 1.50 %,
Temperature 212 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon  (Unverified Data**)
Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve..