Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.65 MPa @Strain 300 % |
530 psi @Strain 300 % |
|
Teknor Apex Telcar® TL-1522A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |