Tensile Stress 0.370 MPa

@Strain 0.160 %,
Temperature 150 °C
53.7 psi

@Strain 0.160 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers