Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 52.74 MPa @Strain 0.430 %, Temperature -20.0 °C |
7649 psi @Strain 0.430 %, Temperature -4.00 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance .. |
|||
Tensile Stress | 52.74 MPa @Strain 0.400 %, Temperature 23.0 °C |
7649 psi @Strain 0.400 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G45HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G45HSL NC010 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide.. |