Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 35.35 MPa @Strain 0.310 %, Temperature -40.0 °C |
5127 psi @Strain 0.310 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de.. |