Mechanical Properties Metric English Comments
Tensile Stress 51.8 MPa

@Strain 2.66 %,
Temperature 23.0 °C
7510 psi

@Strain 2.66 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers