Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 51.2 MPa @Strain 25.4 %, Temperature 23.0 °C |
7430 psi @Strain 25.4 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 51.2 MPa @Strain 0.540 %, Temperature -20.0 °C |
7430 psi @Strain 0.540 %, Temperature -4.00 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 51.2 MPa @Strain 4.16 %, Temperature 60.0 °C |
7430 psi @Strain 4.16 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |