Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 50.9 MPa @Strain 17.8 %, Temperature 23.0 °C |
7380 psi @Strain 17.8 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |