Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.910 MPa @Strain 3.58031 %, Temperature 150 °C |
857.1 psi @Strain 3.58031 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal.. |