Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.77 MPa @Strain 100 % |
837 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® A9885H TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 5.77 MPa @Strain 300 % |
837 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® F02-081A-15B TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |