Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.37 MPa @Strain 0.240 %, Temperature -40.0 °C |
779 psi @Strain 0.240 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010
(Unverified Data**) Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s.. |