Polymer Property : Tensile Stress = 5.33 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 5.33 MPa

@Strain 300 %,
Temperature 23.0 °C
773 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ HC MT224 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT224 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT224 has been specially formulated without the use of any plasticize..
Tensile Stress 5.33 MPa

@Strain 300 %
773 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3875H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..