Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.24 MPa @Strain 200 % |
760 psi @Strain 200 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ EG-9182 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Tensile Stress | 5.24 MPa @Strain 0.100 %, Temperature 150 °C |
760 psi @Strain 0.100 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m.. |