Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.23 MPa @Strain 0.0500 %, Temperature 40.0 °C |
759 psi @Strain 0.0500 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35EF BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubrica.. |
|||
Tensile Stress | 5.23 MPa @Strain 0.0500 %, Temperature 23.0 °C |
759 psi @Strain 0.0500 %, Temperature 73.4 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |
|||
Tensile Stress | 5.23 MPa @Strain 6.30 %, Temperature 0.000 °C |
759 psi @Strain 6.30 %, Temperature 32.0 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |