Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.18 MPa @Strain 100 %, Temperature 23.0 °C |
751 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ CL E85 Thermoplastic Elastomer (TPE) Versaflex™ CL E85 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E85 is also formulated without the use of plasticizer.. |
|||
Tensile Stress | 5.18 MPa @Strain 300 % |
751 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P2880 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 5.18 MPa @Strain 0.100 %, Temperature 100 °C |
751 psi @Strain 0.100 %, Temperature 212 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® LW9330 BK851 PBT
(Unverified Data**) Crastin® LW9330 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |