Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.03 MPa @Strain 300 % |
730 psi @Strain 300 % |
|
NEU NeuSoft™ 455-50A Ester/ether TPU / SBC blend |
|||
Tensile Stress | 5.03 MPa @Strain 0.0500 %, Temperature 23.0 °C |
730 psi @Strain 0.0500 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)
(Unverified Data**) Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed .. |