Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 33.91 MPa @Strain 1.93 %, Temperature 90.0 °C |
4918 psi @Strain 1.93 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 79G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Polyamide 66 Zytel 79G13L NC010 is a 13% glass fiber reinforced toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |