Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 49.04 MPa @Strain 2.25 %, Temperature 90.0 °C |
7113 psi @Strain 2.25 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |