Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 33.64 MPa @Strain 0.330 %, Temperature 0.000 °C |
4879 psi @Strain 0.330 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK549 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Information provided by DuPont Performance Polymers |