Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 48.33 MPa @Strain 0.420 %, Temperature 40.0 °C |
7010 psi @Strain 0.420 %, Temperature 104 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance .. |