Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.28 MPa @Strain 300 % |
475 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Telcar® TL-2470A Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |