Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 32.7 MPa @Strain 21.0 %, Temperature 90.0 °C |
4740 psi @Strain 21.0 %, Temperature 194 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66
(Unverified Data**) Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers |