Mechanical Properties Metric English Comments
Tensile Stress 46.252 MPa

@Strain 0.700 %,
Temperature 23.0 °C
6708.3 psi

@Strain 0.700 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa..