Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 30.725 MPa @Strain 0.500 %, Temperature 0.000 °C |
4456.3 psi @Strain 0.500 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba.. |