Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 30.6 MPa @Strain 45.0 %, Temperature 120 °C |
4440 psi @Strain 45.0 %, Temperature 248 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66
(Unverified Data**) Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 30.6 MPa @Strain 1.06 %, Temperature 120 °C |
4440 psi @Strain 1.06 %, Temperature 248 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |