Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 44.91 MPa @Strain 1.02 %, Temperature 120 °C |
6514 psi @Strain 1.02 %, Temperature 248 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance .. |