Mechanical Properties Metric English Comments
Tensile Stress 30.1 MPa

@Strain 6.00 %,
Temperature 40.0 °C
4370 psi

@Strain 6.00 %,
Temperature 104 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66  (Unverified Data**)
Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers