Polymer Property : Tensile Stress = 43.96 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 43.96 MPa

@Strain 2.00 %,
Temperature -20.0 °C
6376 psi

@Strain 2.00 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I..