Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 29.4 MPa @Strain 0.800 %, Temperature 150 °C |
4260 psi @Strain 0.800 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) 33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provi.. |
|||
Tensile Stress | 29.4 MPa @Strain 0.240 %, Temperature -20.0 °C |
4260 psi @Strain 0.240 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G35HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL NC010 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Tensile Stress | 29.37 MPa @Strain 0.490 %, Temperature 0.000 °C |
4260 psi @Strain 0.490 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G15HSLR BK031 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR BK031 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |