Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.92 MPa @Strain 300 % |
424 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P1860D TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.92 MPa @Strain 100 % |
424 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3960 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |