Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 420 MPa @Diameter 25.0 - 50.0 mm, Strain 0.200 % |
60900 psi @Diameter 0.984 - 1.97 in, Strain 0.200 % |
|
United Cast Bar Unibar 700-2 Continuously Cast Spheroidal Graphite Iron Offers higher wear resistance; strength & heat-treatment response while still possessing reasonable machinability and excellent surface finish. Noise and vibration damping are good in this grade.Uni.. |