Polymer Property : Tensile Stress = 42.04 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 42.04 MPa

@Strain 2.00 %,
Temperature 40.0 °C
6097 psi

@Strain 2.00 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)  (Unverified Data**)
Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also..
Tensile Stress 42.04 MPa

@Strain 8.77 %,
Temperature 23.0 °C
6097 psi

@Strain 8.77 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. ..