Mechanical Properties Metric English Comments
Tensile Stress 28.3 MPa

@Strain 40.0 %,
Temperature 120 °C
4100 psi

@Strain 40.0 %,
Temperature 248 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66  (Unverified Data**)
Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers
Tensile Stress 28.3 MPa

@Strain 0.320 %,
Temperature 23.0 °C
4100 psi

@Strain 0.320 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..