Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 405 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 2.79 MPa

@Strain 100 %,
Temperature 23.0 °C
405 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7670-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7670-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Tensile Stress 2.79 MPa

@Strain 100 %,
Temperature 23.0 °C
405 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7670-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7670-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Tensile Stress 2.79 MPa

@Strain 0.0400 %,
Temperature 40.0 °C
405 psi

@Strain 0.0400 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)  (Unverified Data**)
40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te..
Tensile Stress 2.79 MPa

@Strain 0.0300 %,
Temperature 0.000 °C
405 psi

@Strain 0.0300 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de..
Tensile Stress 2.79 MPa

@Strain 6.00 %,
Temperature 23.0 °C
405 psi

@Strain 6.00 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 2.79 MPa

@Strain 6.87 %,
Temperature 120 °C
405 psi

@Strain 6.87 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET  (Unverified Data**)
47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc..