Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 40.44 MPa @Strain 2.20 %, Temperature 100 °C |
5865 psi @Strain 2.20 %, Temperature 212 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® LW9330 BK851 PBT
(Unverified Data**) Crastin® LW9330 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
Tensile Stress | 40.44 MPa @Strain 1.33 %, Temperature 150 °C |
5865 psi @Strain 1.33 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSLX BK357 is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor.. |