Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.86 MPa @Strain 0.0800 %, Temperature 90.0 °C |
705 psi @Strain 0.0800 %, Temperature 194 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |
|||
Tensile Stress | 4.86 MPa @Strain 16.95 %, Temperature 100 °C |
705 psi @Strain 16.95 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 4.86 MPa @Strain 92.78 %, Temperature 150 °C |
705 psi @Strain 92.78 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |