Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.65 MPa @Strain 100 % |
674 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3780 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 4.65 MPa @Strain 25.0 % |
675 psi @Strain 25.0 % |
Average; ASTM D412 Method A |
Seals Eastern 7265 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Vito.. |
|||
Tensile Stress | 4.65 MPa @Strain 6.90 %, Temperature 100 °C |
674 psi @Strain 6.90 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 4.65 MPa @Strain 6.90 %, Temperature 100 °C |
674 psi @Strain 6.90 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 4.65 MPa @Strain 0.240 %, Temperature 150 °C |
674 psi @Strain 0.240 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 79G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Polyamide 66 Zytel 79G13L NC010 is a 13% glass fiber reinforced toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 4.65 MPa @Strain 11.14 %, Temperature 120 °C |
674 psi @Strain 11.14 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 4.65 MPa @Strain 11.14 %, Temperature 120 °C |
674 psi @Strain 11.14 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |