Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.16 MPa @Strain 25.0 % |
603 psi @Strain 25.0 % |
Average; ASTM D412 Method A |
Seals Eastern 7042U Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Tensile Stress | 4.16 MPa @Strain 60.64 %, Temperature 90.0 °C |
603 psi @Strain 60.64 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |