Mechanical Properties Metric English Comments
Tensile Stress 4.14 MPa

@Strain 300 %,
Temperature 23.0 °C
600 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7431-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7431-1001-00 is an easy processing, performance TPE designed for use in applications requiring a tough, durable material with a low coefficient of friction. - Excellent Heat Stability - ..
Tensile Stress 4.14 MPa

@Strain 200 %
600 psi

@Strain 200 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9172 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun..
Tensile Stress 4.14 MPa

@Strain 300 %
600 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-1336 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Stress 4.14 MPa

@Strain 50.81 %,
Temperature 100 °C
600 psi

@Strain 50.81 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 4.14 MPa

@Strain 98.83 %,
Temperature 150 °C
600 psi

@Strain 98.83 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers