Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 39.84 MPa @Strain 0.290 %, Temperature -20.0 °C |
5778 psi @Strain 0.290 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te.. |