Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 26.87 MPa @Strain 0.230 %, Temperature 0.000 °C |
3897 psi @Strain 0.230 %, Temperature 32.0 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance .. |