Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 26.55 MPa @Strain 0.200 %, Temperature -40.0 °C |
3851 psi @Strain 0.200 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6
(Unverified Data**) 40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 26.55 MPa @Strain 0.200 %, Temperature -40.0 °C |
3851 psi @Strain 0.200 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon
(Unverified Data**) Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve.. |