Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 38.5 MPa @Strain 2.24 %, Temperature 0.000 °C |
5580 psi @Strain 2.24 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6